Engineering Guide · 2 min read
ASTM A320 Grades L7A, L7B, L7C, L70–L73 and L1
A grade lookup for alloy chemistry and impact temperature, including the separate impact-energy requirement for L1.
The short answer. ASTM A320 pairs four alloy chemistries with two standard impact test temperatures. For example, L7C and L73 use the same 8740-type steel, but their standard test temperatures, for sizes requiring a test, are −150 °F and −100 °F respectively. At −100 °F, L1 requires twice the average energy of L70–L73 for the same specimen size. [1]
This grade lookup in the ASTM A320 bolting series covers the less familiar ferritic grades found on drawings and material certificates.
Read across a row to see what changes at the second test temperature. Read down a column to see which alloy the drawing specifies. [1] [2]
| Alloy family and representative steel | Test at −150 °F | Test at −100 °F |
|---|---|---|
| Chromium-molybdenum, 4140 family | L7 | L70 |
| Carbon-molybdenum, 4037 | L7A | L71 |
| Chromium-molybdenum, 4137 | L7B | L72 |
| Nickel-chromium-molybdenum, 8740 | L7C | L73 |
What a 1-in. L72 report tells you about L7B
At 1 in., L7B and L72 have the same minimum tensile and yield strengths, 125 and 105 ksi. Both require a quenched-and-tempered steel. Even the full-size impact energy limits match at 20 ft·lbf for the three-specimen average and 15 ft·lbf for an individual specimen. A report that shows all three energies but omits the test temperature therefore leaves one of the most important fields blank. [1]
If the supplier offers L72 for an L7B order, a standard −100 °F result leaves the −150 °F requirement open. Ask whether the manufacturer can certify the actual lot to the specified L7B grade, with the corresponding impact results and product marking. The 4137 steel designation alone cannot answer that question. [1]
Where Grade L1 fits
L1 is a low-carbon, boron-treated steel with 0.17–0.24% carbon by mass. A320 lists it through 1 in. at 125 ksi minimum tensile strength. For a ¾-in. stud, the distinctive feature is the energy the specimens must absorb at −100 °F. The specimen size must be the same on both sides of the comparison. [1] [3]
| Grade | Average of three | Any one specimen |
|---|---|---|
| L70, L71, L72, L73 | 20 ft·lbf | 15 ft·lbf |
| L1 | 40 ft·lbf | 30 ft·lbf |
A full-size set reading 30, 35 and 40 ft·lbf averages 35. Those illustrative results meet both L70 energy limits but miss the L1 average, even though every specimen reaches the L1 individual floor. For an order marked L1, match both figures to the L1 row. [1]
Stainless low-temperature studs carry B-series designations. For drawings marked B8 or B8M, the next question is which specification and class go with the familiar stainless grade. See ASTM A320 and ASTM A193 Bolting in Grades B8 and B8M.
References
- ASTM A320/A320M-26. Tables 1–4. Strength, Charpy requirements, chemical composition and ferritic grade marking.
- Innovation Fasteners, ASTM A320 Grades L70, L71, L72 and L73. Manufacturer’s data on the paired alloy compositions.
- Innovation Fasteners, ASTM A320 Grade L1. Manufacturer’s L1 chemistry and mechanical data.