Engineering Guide · 2 min read

ASTM A194 alloy steel nuts in Grades 3, 7, 7M, 16 and 43

Identify five alloy steel grades by chemistry and heat treatment, then check whether the order calls for low-temperature impact testing.

November 25, 2026HexFastener

The short answer. Grades 3, 7, 16 and 43 fall in the same heavy hex proof-load column in ASTM A194/A194M-24. They use different alloy compositions. A passing proof-load result alone cannot identify which grade a supplier delivered. Grade 7M shares the chemistry limits of Grade 7 but has a lower proof-load requirement and a hardness ceiling of 235 HBW. [1]

This part of the ASTM A194 nut grade guide covers alloy steel grades and the marks used for impact-tested nuts.

What separates the five grades

GradeAlloy identificationWhat to check before accepting the lot
3Type 501 chromium-molybdenum steelThe chemistry includes 4–6% chromium by mass.
7Chromium-molybdenum steelCheck the grade and heat number even when the bar is described as 4140.
7MShares the Grade 7 chemistry limitsVerify hardness inspection and final stress relief, which a tempering operation can fulfill.
16Chromium-molybdenum-vanadium steelCheck oil quenching and a tempering temperature of at least 650 °C.
43Nickel-chromium-molybdenum steelNickel is a specified constituent. Match the heat analysis to the grade.

The chemistry and heat-treatment comparisons above follow Tables 1 and 2 and Section 6 of the 2024 edition. A tempering temperature describes manufacture. The equipment specification sets the service conditions. [1]

Reading 7L, 7ML and 43L

On a low-temperature carbon steel valve body, Australian Pipeline Valve pairs A320 L7 studs with A194 Grade 7 nuts. For a ¾-inch set ordered to A320, the nut material must meet the impact requirements in the applicable A320 edition. The Charpy test measures the energy a notched specimen absorbs when struck at the specified temperature. A proof-load result alone cannot tell the buyer how the steel behaved in that test. [2] [4]

When the order invokes A194 supplementary requirement S3, Grade 7 follows the A320 L7 impact requirements, 7M follows L7M, and 43 follows L43. A forged Grade 7 nut tested to S3 bears 7L. The corresponding mark on a nut machined from bar is 7BL. Either can identify the specified grade and test. Match the reported test temperature and absorbed energy to the heat-treatment lot. S3 itself exempts bar stock or nuts below ⅝ in. [16 mm] in diameter. [1]

For a joint also subject to sour-service requirements, Grade 7M limits finished-nut hardness to 235 HBW. ISO 15156-2 lists 7M among the acceptable nuts for bolting in its oil and gas production scope. The M identifies the hardness-controlled grade. On a forged 7ML nut, the additional L records impact testing. [1] [3]

For the other material families and their grade guides, see the ASTM A194 grade index.

If the drawing calls for martensitic stainless, see how to distinguish A194 Grades 6 and 6F.

References

  1. ASTM A194/A194M-24. Tables 1–3 and 7, pp. 3–6 and 9. Sections 6 and 8 and supplementary requirements S1, S3 and S10.
  2. Australian Pipeline Valve, Bolting Material ASTM Specifications, revision 5, p. 2. Valve body materials and their stud and nut combinations.
  3. ISO 15156-2:2020, Annex A, §A.2.2.4 and Table A.4. Bolting for oil and gas production equipment in H₂S-containing environments.
  4. ASTM A320/A320M-24a, §1.4 and §10. Nuts for low-temperature bolting and impact-test requirements.