Search HexFastener

Find the part. Understand the spec.

Engineering Guide · 1 min read

ASTM A194 Grades 6 and 6F for martensitic stainless nuts

Grade 6 calls for Type 410. Grade 6F allows two free-machining compositions. Both use the same finished-nut hardness range.

November 25, 2026HexFastener

The short answer. A material certificate that says “400 series stainless” leaves the A194 grade unresolved. Grade 6 uses Type 410. Grade 6F uses a free-machining steel with sulfur or selenium added. All three chemistries make hardenable stainless nuts. [1]

This article in the ASTM A194 series covers the two martensitic stainless nut grades.

Trace the grade to the steel

A194 gradeSteel typeUNS designation
6410S41000
6F416, sulfur-bearingS41600
6F416Se, selenium-bearingS41623

ASTM A194/A194M-24 lists two chemistries for 6F but gives them one grade-and-type entry in the marking table. A purchase specification that restricts the chemistry to Type 416 should carry that restriction onto the order. [1]

What a hardness reading can tell you

Under the 2024 edition, both grades are quenched in liquid or inert gas and tempered. The completed-nut Brinell range is 228–271 HBW for both. A result of 250 HBW would fit either grade. To resolve a disputed delivery, use the lot number on the packaging or delivery note to find the certificate, then check which of the three compositions the steel meets. [1]

If the drawing leaves the material family unclear, use the ASTM A194 grade index to identify it.

For Type 316 and other austenitic nuts, continue with the A194 Grade 8 family and Grade 9C.

References

  1. ASTM A194/A194M-24. Tables 1–3 and 7, pp. 3–6 and 9. Sections 6 and 8 and supplementary requirements S1, S3 and S10.