Search HexFastener

Find the part. Understand the spec.

Engineering Guide · 2 min read

ASTM A320 Grade L43 for Large-Diameter Studs

Why L43 comes up on a 3-inch stud order even though L7 carries the same strength and impact requirements in its usual size range.

November 25, 2026HexFastener

The short answer. On a 3-in. low-temperature stud, ASTM A320 Grade L43 brings the same 125 ksi minimum tensile strength specified for smaller L7 studs into a larger listed diameter range. L43 is a nickel-chromium-molybdenum steel. Its usual size advantage comes from its ability to harden deeper into a thick section during quenching. [1] [2]

This article in the ASTM A320 bolting series looks at what changes when a flange needs a larger stud.

Compare the strength and impact requirements first. The two grades carry the same minimums. The listed diameter is where they differ. [1]

Inch-series studs under ASTM A320/A320M-26, Tables 1 and 2. Impact values are for 10 × 10 mm specimens.
RequirementL7L43
Listed diameterThrough 2½ in.Through 4 in.
Minimum tensile / yield strength125 / 105 ksi125 / 105 ksi
Charpy at −150 °F20 ft·lbf average, 15 individual minimumSame

ASTM’s size footnote matters at the quotation stage. It describes the largest commonly available sizes that consistently met the requirements. If the drawing calls for L7 above 2½ in., ask for results covering the ordered diameter and heat-treatment lot. A report for 2-in. L7 bar alone does not establish the properties of a 3-in. stud. [1]

Where to take the impact specimen in a large bar

The center of a large bar cools more slowly than the surface during a quench. A steel with greater hardenability can develop the required hardened structure farther into the bar before tempering. L43 uses a 4340-type chemistry with 1.65–2.00% nickel by mass. Its maximum specified hardness is still 321 HBW, the same as L7. The benefit here is how far the steel hardens across the section. [1] [2]

A320 locates impact specimens at the axis for sections 1 in. or smaller, and midway between axis and surface for sections over 1 in. In a 3-in. round section, that second location is ¾ in. from the center. A surface hardness reading and a Charpy result from that location describe different properties at different depths. [1]

Cross sections of 1-inch and 3-inch bars. Impact specimens are centered on the axis of the smaller bar and halfway out along the radius of the larger bar.
Impact specimen locations in round sections under ASTM A320/A320M-26 §6.2.3. In the 3-in. example, half the radius is 0.75 in. [1]

When the drawing adds lateral expansion

A 4340 chemistry callout alone leaves the impact result open. ASTM specifically notes that meeting the L43 requirement at −150 °F can call for tighter control of phosphorus and sulfur than commercial 4340 normally receives. Ask for results representing the ordered diameter, heat and heat-treatment lot. [1]

Look also for supplementary requirement S2. If the order invokes it, the laboratory measures how much the broken specimen widened on the compression side. Each specimen must show at least 0.015 in. of lateral expansion at the temperature specified by the purchaser and agreed with the manufacturer. This dimension is additional to the absorbed energy. A report giving only ft·lbf leaves the S2 requirement unanswered. [1]

A drawing marked L7C or L73 can also point to nickel-chromium-molybdenum steel. Those grades have their own compositions and test temperatures. They are compared in ASTM A320 Grades L7A, L7B, L7C, L70–L73 and L1.

References

  1. ASTM A320/A320M-26. §1.2, Tables 1–3, §6.2.3 and supplementary requirement S2. Size footnote, impact specimen location and lateral expansion.
  2. Innovation Fasteners, ASTM A320 Grade L43. Manufacturer’s material data for 4340 chemistry and hardenability in large sections.